before i get started on my problem,was it just me or was the site of line for over a week ?was really uptight as i couldnt get in and see what was going on.
now.....my problem is with stannous testing.
ive bought pure chloride off ebay and followed the instruction from one of the books or recipes ive downloaded in various pdf files.
it instructs 2 grams of powder in 35 mil of hcl is this right?as i then found another one that said to put a small piece of tin metal in the mix?
now i need this to be right or else im not testing mixtures correctly that could still have gold content,and then maybe throwing away as waste.
can anyone help?
 
superten,

While I haven't had any problem recently, I have had problems accessing the forum a couple of times. There are a few threads in the Technical Problems with the Forum Site category. Here are a couple:

http://goldrefiningforum.com/phpBB3/viewtopic.php?f=64&t=14799

http://goldrefiningforum.com/phpBB3/viewtopic.php?f=64&t=12250

Really causes a PANIC when it happens, doesn't it?!

Dave
 
lol yeah im allways on here reading and looking at pics of people inventions etc i love it.
 