budzag
Active member
Also what is the ideal pH to cement gold? Why would adding more ammonia rise the pH you would think ammonia would be acidic and would lower the pHThanks, I am aware of this I have a tinny little bead of gold that I will test on to see if I can get it dissolved in solution. The starting list will be 1/4 tea spoon of copper sulfate, then I will add 3 tea spoons of sodium thiosulfate, then i will add 3 tea spoons ammonium sulfate and then I will use ammonia as the liquid no water will be added. Will let it sit for a few days then will check the result and see if the bead is reducing in size.