giom said:
from all this how you precipate gold from colloidal sessponsion and make it back to metal .
Translated...
giom said:
From all this how do you precipitate gold from colloidal suspension and make it back to metal?
Firstly, colloidal gold is also gold at oxidation state 0, in other terms metallic gold just as any gold nugget or coin. It might be covered by a layer of charged particles that repels the clusters so they don't coalesce into particles large enough to sediment at the bottom.
So to return colloidal gold into something more dense you can basically do it in three different ways
1. Melt it. First dry out the suspension so you get a gold powder. When the solvent is gone the gold will be close enough so heat can break down the barriers between the particles.
2. Break down the surface that keeps the particles apart. Possible boiling in an acid or base. Will be specific depending on how the colloidal gold were prepared.
3. Dissolve in aqua regia and precipitate with standard methods.
I've only tested the third method. Made some beautiful red gold solution by adding stannous to gold chloride. A bit more AR turned it back into gold chloride and I precipitated it in normal ways.
Giom, if your "gold" doesn't melt then it isn't gold. No matter how much you really want that your house is built on top of a gold mine, the simple explanation is that it isn't.
If you comes to term with what you have learned about ormus gold... and everything else you wrote above is just plainly wrong then you can start to learn real refining, where we regularly take material where one out of a thousand atoms is gold and turn it in a pure form where one out of a thousand atoms is not gold. And we barely misplaces any atoms on the way.
Anyone following the ormus gold and alchemy way is turning their back against 500 years of scientific development and is missing the real magic.
Giom, a warning. This forum is based in science and not fairy tales, continuing to defend ormus gold and other alchemy will get you banned in the end.
By the way, what did stannous test show?
Göran