• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

Chemical Using Zinc to deal with Tin Oxide from dirty Copper Chloride etches- experiment writeup

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

haveagojoe

Well-known member
Joined
Aug 1, 2014
Messages
351
I use Copper Chloride etching on a wide range of source material, including plated connectors, pins (incuding magnetic ones) and all kinds of other plated or flashed escrap. This means my collected foils are often quite heavily contaminated with other metals.

Also I tend to aggitate my etches quite aggressively by shaking, so my foils are often broken down into finely divided black powder. Black powder also forms when gold is dissolved and cemented back out, for example when hydrogen peroxide is added (though I don't do this any more).

Tin oxide is a particularly annoying contaminant to find among my foils- a white precipitant which looks similar to Copper (I) Chloride but will not redissolve with the addition of fresh HCl. It's difficut to separate from the foils, and furthermore it can hydrolyze to form the dreaded metastannic acid, which in water is a jelly-like substance which can trap gold and is very challenging to deal with. Ideally foils should be as free of other metals as possible - particularly tin- prior to dissolving, in order to ensure best purity of the refined gold powder and to avoid complications.

Other contaminants can include Iron and Nickel oxides - which appear as fine black or brown powders (mud), which can be mixed with (and mistaken for) finely divided gold.

The common approach to dealing with tin oxide has been to roast the foils, in order to convert it to soluble tin compounds, and wash again in HCl prior to refining. I have never really been convinced by the effectiveness of this approach and it's a bit of a pain to do.

I came across an alternative approach: to convert Tin Oxide to soluble Tin (ii) Chloride by reduction using Zinc. In a post-etch cleanup of the foils with fresh HCl this allows Tin to be separated from the foils by filtration.

SnO2+Zn+2HCl→SnCl2+ZnO+H2↑

Zinc Oxide is also soluble in HCl, forming Zinc Chloride, so would be in liquid phase and would pass through the filter.

ZnO+2HCl→ZnCl2+H2O

Using Zinc would also have the advantage of reducing Nickel oxide and Iron oxides to soluble Nickel and Iron chlorides:

Fe2O3+Zn+6HCl→2FeCl2+ZnCl2+3H2O

NiO+Zn+2HCl→NiCl2+ZnO+H2↑


I performed an experiment, dissolving the zinc casings of two AA batteries in about 300ml of fresh 10% HCL in a beaker which contained my foils and black powder, and a layer of white tin oxide contaminant.

Zinc powder would be ideal for this approach but it's expensive, and I found that the zinc battery casings were quite adequate and even though I did not cut them into small pieces they dissolved completely within about 5 minutes. The resulting hydrogen produced quite a head of froth as my HCl is store-bought muriatic acid which contains a foaming agent- I was able to knock it down with a spray bottle.

After stirring for a futher 10 minutes the Tin oxide appeared to have been successfully converted to soluble Tin Chloride as no white mud was visible. The solution was very dark brown, almost black, loaded with the suspended black powder - which, since Iron oxides and Nickel oxide should also have been reduced to soluble chlorides, should now consist only of finely divided gold.

I let the solution settle for about an hour, but it was very slow to settle and remained almost black. So I decanted the solution off the layer of settled foils and black powder, through a coffee filter. The tin chloride can still hydrolyze to form metastannic acid so I wanted to separate it from the bulk of the foils as soon as possible. A lot of the suspended particles were too fine to be caught by the filter; the filtrate remained dark so I left it to settle further.

The gold foils had turned pink at this stage- evidently some copper was present had cemented onto them. I added fresh HCl to the beaker of foils, which quickly appeared to redissolve the copper, restoring their normal gold colour.

The filtration will take a long time, and both the filtrate and the beaker of foils will likely take a day or two to settle, but at this stage I am quite confident that this approach has successfully dealt with the Tin oxide, as well as Nickel and Iron oxides. If it proceeds as expected, I intend to go straight to dissolving the foils with fresh HCl and pool chlorine tablets, without the need for roasting.

I will update this thread as the experiment concludes.
 
Last edited:
I never personally dealt with tin oxy-chlorides in my whole refining career while using AR as my primary method. Though I cannot say for sure if this also applies for AP - where tin can be present in lower (II) oxidation state, rather than Sn(IV) as it is in AR solutions.

But my hints:

1. Metastannic acid "pain" is glorified in my opinion. Yes, it is slow to filter with regular methods, but with Buchner, piece of plastic mesh and real filter paper (not coffee filters) - not that problematic anymore. Also, you can advantageously use some filtering aid such as Celite or bentonite.
When I compare metastannic from say nitric leaches with say crushed MLCCs leached disintegrated ceramics - I would rather pick to filter metastannic suspension 10x than once dealing with disintegrated cerams.
Not saying it isn´t beneficial to look for alternatives, but good old filtration may be the best option.

2. If you maintain acidic enviroment, there should not be any nickel or iron hydroxides/oxides/oxohydroxides. When enviroment of leach is deprived of acid - which provide stabilizing counterions to dissolved metal - only possible option is to take the anion from water :) So top it up with some HCl and you will be good to go.

3. If you want to produce zinc powder, buy zinc oxide. Prepare strong NaOH solution (say 20 % will be OK) and saturate it with zinc oxide - add comfortable excess so it settle to the bottom. Then, electrolyze this solution using nickel electrodes (you can try quality stainless steel like 316, but I always used nickel). Zinc would grow as spongy fluffy deposit, which barely hold together - but if you don´t knock it off, it holds even if 1,5cm thick. When there is nice layer of the zinc, remove the electrode and crumble the deposit into container with water. You need to wash it relatively quickly because when disconnected, zinc would be eaten back up by hydroxide.
Easily scaleable, just need some fiddling with current and voltage - when you reduce hydrogen, lower the voltage until it just stop bubbling (as with nearly all electrolysis from solutions). The prepared zinc is very active - I would sometimes say too active.

4. From my experience, hydrolysis of tin chloride is acid-dependant. Much much more, than time-dependant. If you want to avoid hydrolysis, wash with some dilute HCl - at least 3M HCl (10 %) was nearly always effective to practically stop the hydrolysis.
I found this when I prepared stannous chloride solution from old, partially hydrolyzed SnCl.2H2O which I have in the lab. When done with water or say weak 1-2 % HCl, cloudiness was very evident and persistent. When I dissolved these white powdery decomposed crystals in say 3M HCl, I obtained slightly milky solution which cleared quickly (particles settled nicely).

Another good source of high zinc alloy are wheelweights - at least here in EU, where we have strict regulations and lead was phased out due to enviromental pollution reasons.

I am looking forward for more good experimental work :)
As it is said frequently: Difference between messing around and doing science is properly writing up everything :)
 
Thanks Orvi!
Metastannic acid "pain" is glorified in my opinion.
I agree, I was being a little hyperbolic. I only encountered it once and I basically just ignored it, but I think tin carried through into my melt.
there should not be any nickel or iron hydroxides/oxides/oxohydroxides
Yes, you're right, they should stay in solution. I am just surprised at the amount of black powder and couldn't trust that it's all gold! Perhaps I should kick my habit of shaking up my etches, it breaks the foils up so small they take forever to settle.

produce zinc powder, ....
The prepared zinc is very active - I would sometimes say too active.
Yes, after seeing the speed which the battery casings dissolved, I think I will not need to use zinc powder, I think it could produce quite a violent reaction.
hydrolysis of tin chloride is acid-dependant. Much much more, than time-dependant.
Yes I think that must be true too. The one time I encountered it was when I stored foils in plain water for several weeks. But nowadays I can only get 10% HCl, so if I use the spray bottle it gets diluted even further, maybe to a point where hydrolysis could start if I left it too long.
 
2. If you maintain acidic enviroment, there should not be any nickel or iron hydroxides/oxides/oxohydroxides. When enviroment of leach is deprived of acid - which provide stabilizing counterions to dissolved metal - only possible option is to take the anion from water :) So top it up with some HCl and you will be good to go.
Perhaps insoluble oxides of Nickel and Iron may form because of using an air bubbler in the Copper Chloride etch? Oxidizing directly with O2 rather than taking an anion from the H2O. I think you're right that the solution is not sufficiently acidic to keep the Nickel and Iron dissolved as chlorides, but since the acid I can buy is only 10%, I think unfortunately adding more of it may not help much.

I should use HCl in the spray bottle rather than water though, that should help to prevent further dilution.
 
Last edited:
Perhaps insoluble oxides of Nickel and Iron may form because of using an air bubbler in the Copper Chloride etch? Oxidizing directly with O2 rather than taking an anion from the H2O. I think you're right that the solution is not sufficiently acidic to keep the Nickel and Iron dissolved as chlorides, but since the acid I can buy is only 10%, I think unfortunately adding more of it may not help much.

I should use HCl in the spray bottle rather than water though, that should help to prevent further dilution.
10 % HCl should be OK for this. Generally, iron start to precipitate around pH of 4 (in dilute solutions).

This is strange concentration for purchase. Where are you located ? Even here in EU there is no problem getting regular techgrade 30% HCl even in regular consumer stores.
 
Where are you located ?
UK. Things have got quite tight here, nitric is not available without a licence and there is a limit for peroxide too at 12%, and if you buy it at a pharmacy they may ask you to fill in a questionnaire. I buy HCl as concrete cleaner but even that is getting more difficult as alternative preparations are becoming more widely used in the product.
 
UK. Things have got quite tight here, nitric is not available without a licence and there is a limit for peroxide too at 12%, and if you buy it at a pharmacy they may ask you to fill in a questionnaire. I buy HCl as concrete cleaner but even that is getting more difficult as alternative preparations are becoming more widely used in the product.
Nitric and peroxide are on the license only for whole EU. But HCl isn´t restricted... Is it restricted in UK too ? Or just nobody small around you offer this to regular person like us ?
If there wasn´t HCl available at regular household stuff shops/chemist´s, I can still purchase from some smaller local sellers of chemicals. Against ID, you can buy anything non-restricted here. Many of these companies do not have e-shops or physical stores with opening hours. But once you call the guys, say I need a canister of tech grade 30% HCl for cleaning, have my ID and pay cash... I think you will find somebody willing to sell :)
Or find someone with business license to buy it for you... HCl is dirt cheap.
 
HCl isn´t restricted... Is it restricted in UK too ?
Yup :(

The Control of Poisons and Explosives Precursors Regulations 2023:

The Following Substances Are Classified as Regulated Explosive Precursors:
Ammonium Nitrate 16% N
Nitromethane 30% W/W
Potassium Perchlorate 40% W/W
Hexamine
Nitric Acid 3% W/W
Sodium Chlorate 40% W/W
Hydrochloric Acid 10% W/W
Phosphoric Acid 30% W/W
Sodium Perchlorate 40% W/W
Hydrogen Peroxide 12% W/W
Potassium Chlorate 40% W/W
Sulfuric Acid 15% W/W
 
Yup :(

The Control of Poisons and Explosives Precursors Regulations 2023:

The Following Substances Are Classified as Regulated Explosive Precursors:
Ammonium Nitrate 16% N
Nitromethane 30% W/W
Potassium Perchlorate 40% W/W
Hexamine
Nitric Acid 3% W/W
Sodium Chlorate 40% W/W
Hydrochloric Acid 10% W/W
Phosphoric Acid 30% W/W
Sodium Perchlorate 40% W/W
Hydrogen Peroxide 12% W/W
Potassium Chlorate 40% W/W
Sulfuric Acid 15% W/W
I guess this even regulate what you have not just what you can buy?
So if you increases concentration it will be illegal?
 
In my limited knowledge of how explosives are made, I fail to see where HCl fits into this list.

To me, this list looks more like how to make lives hard for anyone with a benign legitimate use of these chemicals, than a way to stop terrorists or criminals.

Edited to remove section that could be misunderstood
 
Last edited:
Yup :(

The Control of Poisons and Explosives Precursors Regulations 2023:

The Following Substances Are Classified as Regulated Explosive Precursors:
Ammonium Nitrate 16% N
Nitromethane 30% W/W
Potassium Perchlorate 40% W/W
Hexamine
Nitric Acid 3% W/W
Sodium Chlorate 40% W/W
Hydrochloric Acid 10% W/W
Phosphoric Acid 30% W/W
Sodium Perchlorate 40% W/W
Hydrogen Peroxide 12% W/W
Potassium Chlorate 40% W/W
Sulfuric Acid 15% W/W
get one of these and a bucket of salt. If H2SO4 is hard to get, demolish some car batteries. Then use potassium or ammonium nitrate in stead of the salt, and you can make nitric.
https://www.ebay.co.uk/itm/126636334975
 
Experiment update: dissolution of the foils with HCl+pool chlorine tablets is not going as expected.
Although I presoaked in HCl, the pink colour I observed on the foils earlier had apparently not dissapeared, it was visible when I stirred the beaker with the addition of chlorine tablet dust. The foils are not dissolving. I thought maybe the pH had gone up so I added more fresh HCl, still no dissolution. I added more tablet dust, still no dissolution. I tried adding a little household bleach to no effect. Neither the black powder nor the visible foils are dissolving. After waiting a little for the black powder to settle the top layer of the solution is dark green, so I think there must be a lot of copper chloride and possibly nickel chloride in solution.

I have left it covered with plastic film to keep the chlorine in while I figure out what to do. I think some copper has cemented onto the foils and somehow passivated them maybe. Or the Zinc has affected things in some other way. I'm annoyed because last time I used these tablets it worked perfectly.

I think probably the best course of action will be to let it settle, decant off the solution and try again with fresh HCl. There may be some gold dissolved in the solution though so I guess I'll try to cement it out.
 
Stannous tests reported no gold in solution, so I decanted the solution and washed the solids with HCl. The washes are coming out pale blue and the remaining solids are grey-black sludge with foils mixed in. My current theory is that the majority of the black powder was not finely divided gold but rather copper, nickel and iron oxides which consumed the chlorine as they turned back to chlorides, and are now in the green decanted solution- there should be a strong smell of chlorine still, but there is none.

Ah well, this all started out as a dirty etch and only got more messy, I'll have fun sorting it out and eventually will learn something from it I hope :)
 
Update:
After washing the solids several times wih HCl until the green-blue colour disappeared, I made a second attempt at dissolving the foils and this time was successful.

I was concerned that perhaps powdering the tablet had meant the chlorine escaped too quickly- it seemed to react quickly on the surface with a lot of fizzing and foam. So on the second attempt I opted to use 2.5g of tablet in a single chunk. This meant the tablet was very slow to dissolve; it took several hours of stirring (manually!) but I was confident that very little chlorine escaped since there was hardly any smell, and eventually all the foils did dissolve. After settling I now have a beaker of nice golden-orange coloured solution with only dross and white tablet filler at the bottom.

Since I think there could be other metal chlorides in the solution as well as the gold, after filtering I think I'm gonna cement with copper rather than dropping with SMB.

I'm still not clear as to what caused the issue the first time- whether the zinc or other metal oxides interfered with the dissolution, consuming chlorine; whether the zinc caused cementation of copper which created a passivating layer on the foils; or whether powdering the tablet was the problem. I've used the tablet in powdered form before with great success so I do think the contamination was mostly to blame.

The main thing I have learned is that black powder is not just finely divided gold foils, it can also be other metals in the form of oxides, and I think the cause of that is the combination of over-oxidation with the bubbler and the low concentration of my HCl.

in solution.jpg
 
Last edited:
Update:
After washing the solids several times wih HCl until the green-blue colour disappeared, I made a second attempt at dissolving the foils and this time was successful.

I was concerned that perhaps powdering the tablet had meant the chlorine escaped too quickly- it seemed to react quickly on the surface with a lot of fizzing and foam. So on the second attempt I opted to use 2.5g of tablet in a single chunk. This meant the tablet was very slow to dissolve; it took several hours of stirring (manually!) but I was confident that very little chlorine escaped since there was hardly any smell, and eventually all the foils did dissolve. After settling I now have a beaker of nice golden-orange coloured solution with only dross and white tablet filler at the bottom.

Since I think there could be other metal chlorides in the solution as well as the gold, after filtering I think I'm gonna cement with copper rather than dropping with SMB.

I'm still not clear as to what caused the issue the first time- whether the zinc or other metal oxides interfered with the dissolution, consuming chlorine; whether the zinc caused cementation of copper which created a passivating layer on the foils; or whether powdering the tablet was the problem. I've used the tablet in powdered form before with great success so I do think the contamination was mostly to blame.

The main thing I have learned is that black powder is not just finely divided gold foils, it can also be other metals in the form of oxides, and I think the cause of that is the combination of over-oxidation with the bubbler and the low concentration of my HCl.

View attachment 67502
Nice color.
 
The colour looks a bit more normal after filtering, dropping out the lead with sulfuric, and then double filtering again. Maybe it was just the lighting.

I tend to get impatient at this stage and use an excess of SMB rather than off-gassing the chlorine properly. But this time there's no point rushing as I'm waiting for a new crucible to arrive anyway so I'll just wait. I think I ought to cement it really but the excitement of seeing it drop with SMB is very alluring :)
 