To me, it appears as Vermeil jewelry and as such it would be a 2.5 micron layer of 10K gold plating over Sterling silver. So it's worth it's weight in Sterling.
Hi Thomas!To me, it appears as Vermeil jewelry and as such it would be a 2.5 micron layer of 10K gold plating over Sterling silver. So it's worth it's weight in Sterling.
If I buy it I'll post the answer.You have me curious...
Happy Holidays
That's the whole piece if it helps.If I recall correctly, vermeil will be stamped 925 (occasionally 999). since it is always gold plated over either sterling or fine silver. I don't recall ever seeing a piece with a karat stamp, since 10K is almost always used by reputable makers for the best resistance against wear and tear of the plating.
Vermeil pieces are usually well made, which makes me a bit suspicious of this piece, as the beads do not seem to be formed well at the openings.
If you buy it from a guy in an alley wearing a heavy trenchcoat... it's probably totes legit! ;DI have never seen that mark. Just remember that there are scammers who stamp 14 and 18K on alloys of Copper, Zinc, and Tin. Not even a flash of Au plating. Buyer be weary. He could be passing on something not legit, by stating the obvious in the hallmark, especially if he says he doesn't know what it is. Not a deal I would care to be involved in. But chalk it up to experience, if you get burned. Like others said, if it is too good to be true, it probably is.
From the picture of the close up, it looks like either the plating is separating, or a poorly crafted bead form. Maybe have him/her send 1 bead to you for testing.That's the whole piece if it helps.
I have to say I am happily surprised by the number of replies to my question.i’m a jeweler. The construction of the male end clasp suggests its costume. It possibly could be karat gold but i don’t think so. Trust but verify.
If you have the money to gamble it’s up to you , buy it figuring it is not gold and be happy if it is.