Cool thanks.get the 1" size, it will give you more CFM.
Cool thanks.get the 1" size, it will give you more CFM.
delboy9891, I could suggest a vacuum valve, you need a vacuum however a slight reduction in vacuum may slow the velocity of the fume going through your system. In my situation, we are installing Column Scrubbers with Glass Barrel media to slow down and diffuse the fume.Easy enough to put a vacuum guage on it, like I said this will be the most important piece of equipment I will ever have, safety first, the other thing I am studying at the moment is safely dealing with the waste, when I am confident of that only then will I start refining
you can neutralize any waste to pH of 7Easy enough to put a vacuum guage on it, like I said this will be the most important piece of equipment I will ever have, safety first, the other thing I am studying at the moment is safely dealing with the waste, when I am confident of that only then will I start refining
Yes after having dropped most of the Hydroxides.you can neutralize any waste to pH of 7
Those are nice columns, how tall are they? As suggested a vacuum valve to slow down the airflow to better match the flow generated by the eductor with the size of the column. Remember the retention time for the fume in the column is what makes this work. And all glass gives the advantage of seeing the color of the fume to determine when you need new chemistry.we are installing Column Scrubbers with Glass Barrel media to slow down and diffuse the fume.