Welcome to us.Hi
Name: sandeep located in vancouver Canada. I have electronic scrap. I am curious to turn into gold but stuck at buying nitri acid. Unable to find it. I already read hoke book.
Thank u
Thank. I will try hcl and bleach method. Am I am second though was that.Welcome to us.
You can easily refine Gold from electronics without Nitric.
Dissolving thin Gold can be done with HCl/Bleach, HCl/Chlorine or HCl/Peroxide for example.
Just be careful, small aditions and often pH checks.Thank. I will try hcl and bleach method. Am I am second though was that.
I didn't understand when finished drop it appr 1-2.. can u please explain me.Just be careful, small aditions and often pH checks.
The pH should not get higher than 4-5 and when finished drop it appr 1-2.
When your adding bleach your ph will change. (Higher possibly 4-5)I didn't understand when finished drop it appr 1-2.. can u please explain me.
Thank u
Base merals are removed first, before going for the Gold.I have a question like what about base metals. Doesn't it involve with dissolving gold
Is there any way.. to remove base metals without using nitric acid.. because hard to get nitric acid in vancouver..Base merals are removed first, before going for the Gold.
Yes, search the forum for AP or Cupric Chloride leach.Is there any way.. to remove base metals without using nitric acid.. because hard to get nitric acid in vancouver..
You can learn it all here, but please study and ask before you try anything.Is there any way.. to remove base metals without using nitric acid.. because hard to get nitric acid in vancouver..