The pentium MMX chip you show they pay 83 cents per chip. 8)
plamenppp said:Not bad at allI can buy the green ones for less than 0.1 USD per piece and I can have motherboards for free.
plamenppp said:Notice taken. I apologize for my language but I was too excited.
Today I found some more of these "ИЗОТ" parts. About 10 kg. The cost me a bottle of bier - 2 L.
Black and white TVs are also a good place to find some precious metals. I should post some pictures.
teclu said:plamenppp said:Notice taken. I apologize for my language but I was too excited.
Today I found some more of these "ИЗОТ" parts. About 10 kg. The cost me a bottle of bier - 2 L.
Black and white TVs are also a good place to find some precious metals. I should post some pictures.
Can you make a few pictures with TV boards where these golden transistors are mounted?
You have 10Kg of these parts?
In your picture, in the left side, are some AgPd cursors from russian potentiometers?
teclu
plamenppp said:Yes, teclu. It is written PtKd on them. I am gathering more of them now. And on the second picture everything is from Bulgaria. There might be some russian parts and chps but they are not many. I still can not find a big calculating machine "ЕЛКА" (some of the parts on the second pictures are from there). I know that inside there is as much Au, Ag, Pt and Pd as to buy a four room apartment. Probably someone else has known this in 1989 when the communism felt down and chaos began ...
gorfman6154 said:plamenppp, now that's more like it, the gold plated transisters run around $180-$200 a pound.
As in mining, you want to high grade, or get the good parts. Cpu's, fingers, pins, and other gold plated components. Your starting to get a good eye for your e-scrap.
Those transisters, after you snip them open, work very nicely in Lazersteve's stripping cell.
Good luck, Gorfman.
plamenppp said:Telcu, is the potentiometer the square part with the circle on it and the long rectangle part? The have place for a small screwdriver on them. I have 10 of the square ones from 2 Pravetz's monitors. They have a small thin metal circle inside - Pd 600 (60% Pd). Pleace, telcu, if you have time and wish draw some red circles on my pictures and post them![]()