Ahk
Well-known member
Ok cool thank you so much I’m almost home so I can show you betterJust enough to get it properly liquid again. A few ml, maybe 10 or so.
Ok cool thank you so much I’m almost home so I can show you betterJust enough to get it properly liquid again. A few ml, maybe 10 or so.
That is enough to dissolve 5 grams of pure Gold.Barely any just enough to dissolve it was 5ml
None I didn’t add it at allThat is enough to dissolve 5 grams of pure Gold.
How much Urea did you use?
I misread you.None I didn’t add it at all
Oh I’m sorry, I didn’t add urea at all just smbI misread you.
Nothing to be sorry about.Oh I’m sorry, I didn’t add urea at all just smb
Thank you for your help here is a pic of the stannous test I just didNothing to be sorry about.
But you probably have an excess of Nitric in your solution.
Add a piece of Copper and cement it out or evaporate to remove excess Copper as said earlier.
It seem positive, yes.Thank you for your help here is a pic of the stannous test I just did
We need to update these pics Ygg. Yes they work but could be improved. Maybe different strengths of result and add the false report colours on one thread?