OK UPDATE!!!

I went to chesk the solution to see if it still fizzed when adding SMB.

Resoult is... it dosent

I see some brown powder at the bottum of the solution, however the solution is gloden brown.

Should i add more SMB to the solution after already adding some?

and

should it be be added as is ( salt crystals) or mixed with H20 also what happens if the solution remains the same color? I realize SMB should be added acording to the ratio of gold.

thanks,
 
Patience.
I wouldn't add any more then a teaspoon of SMB as you didn't sound like you had much gold to begin with.