kadriver
Well-known member
I bought one of Steve's dvds called Silver A to Z.
One of the segments was on recovering silver metal from SILVER CHLORIDE.
I had about 4000 ml of clear dark blue liquid left over from refining some silver.
I squirted hydrochloric acid a ldropper full at a time until no more silver chloride would precipitate.
I let all the containers settle and poured off the liquid into my waste container.
I then combined all four containers of silver chloride that I had precipitated in one container.
Using hot water, I washed the silver chloride over and over.
This washing reduced the amount of silver chloride.
I think the washing got rid of some water solubles that were not silver chloride.
Once the silver chloride was washed and the water was clear of all color I followed the procedure on Steve's dvd.
I could not believe my eyes when I added SUGAR to the mix and silver began to form in the container!
I got an ounce of pure silver metal from the 4000ml of liquid. i was wondering what I was going to do with it.
Steve's dvd paid for itself the first day I got it - THANKS STEVE!
One of the segments was on recovering silver metal from SILVER CHLORIDE.
I had about 4000 ml of clear dark blue liquid left over from refining some silver.
I squirted hydrochloric acid a ldropper full at a time until no more silver chloride would precipitate.
I let all the containers settle and poured off the liquid into my waste container.
I then combined all four containers of silver chloride that I had precipitated in one container.
Using hot water, I washed the silver chloride over and over.
This washing reduced the amount of silver chloride.
I think the washing got rid of some water solubles that were not silver chloride.
Once the silver chloride was washed and the water was clear of all color I followed the procedure on Steve's dvd.
I could not believe my eyes when I added SUGAR to the mix and silver began to form in the container!
I got an ounce of pure silver metal from the 4000ml of liquid. i was wondering what I was going to do with it.
Steve's dvd paid for itself the first day I got it - THANKS STEVE!