patnor1011 Well-known member Joined May 22, 2008 Messages 4,259 Location limerick Jan 31, 2012 #41 No problem. It looks that RAM chips yield will be in region of 2g Au from kilogram. Or 1g from lb. That is pretty much the same I got from last batch.
No problem. It looks that RAM chips yield will be in region of 2g Au from kilogram. Or 1g from lb. That is pretty much the same I got from last batch.
philddreamer Well-known member Joined Feb 12, 2010 Messages 2,276 Location Lynnwood, WA. Feb 1, 2012 #42 That's good to know, I won't try to squeeze any more out of my batch! :mrgreen: Pat, did your batch test + for Pd?
That's good to know, I won't try to squeeze any more out of my batch! :mrgreen: Pat, did your batch test + for Pd?
patnor1011 Well-known member Joined May 22, 2008 Messages 4,259 Location limerick Feb 1, 2012 #43 Yes, I do have picture somewhere home, my chips were mixed, from RAM sticks but pretty much all types and ages imaginable.
Yes, I do have picture somewhere home, my chips were mixed, from RAM sticks but pretty much all types and ages imaginable.