Hey there Nevadans Im in vegas! I need advice on buying those pre melted compuer scrap blocks or bars and taking them to Elemetal here in town for refining. Is that worth it? Can you advise on ebay sellers you have used? What is the purity of those melted compouer ram chip prongs, etc?
Don't! it's a scam!
There is no gold.
Elemetal may not even bother to assay it.

Why would anyone sell scrap over internet when almost every scrap dealer knows the value of E-waste?
Look for scrap buyers on the internet and look at what the give for certain e-waste.

Because on the internet you can't see the product and they can present it as something high value, seed the top with shiny items and suckers fall for it.

All molten computer pin "golden bars" are a scam! each and every one them.
Never buy any of it and report each seller as a scammer to the platform they are on.

No e-waste seller on Ebay or any internet site is real! they only sell it there to scam people.
Ebay does not seem to care and keeps facilitating these scams to take place, but obviously, as long as they're making money, they're happy and don't care people get scammed and then start polluting the environment with chemicals as they try to find gold that is not there.

Thanks E-bay for contributing to polluting our beautiful planet!

I hope they will be held responsible one day!
What was their sustainability standpoint again?
 
Hey there Nevadans Im in vegas! I need advice on buying those pre melted compuer scrap blocks or bars and taking them to Elemetal here in town for refining. Is that worth it? Can you advise on ebay sellers you have used? What is the purity of those melted compouer ram chip prongs, etc?
No these pre-melted e-scrap blocks are not worth anything, it will cost way more to process them than there is Gold in them.
 
Hey there Nevadans Im in vegas! I need advice on buying those pre melted compuer scrap blocks or bars and taking them to Elemetal here in town for refining. Is that worth it? Can you advise on ebay sellers you have used? What is the purity of those melted compouer ram chip prongs, etc?
Sorry, where is my manners.
Welcome to us, but these blocks are as Martijn said almost guaranteed, scam.
 
I’ll weigh in on this. I bought 40 LBs of processors on eBay and only recovered 4 grams. It turned out the lands had been mixed with tungsten. Good luck with that website!
 
Hello, there is a company that provides a waste testing service for gold concentration, you can send them 1 chip for testing before you purchase a large amount
 
Last edited by a moderator:
If you want to advertise for your company, you need to do it in the Vendors - Refiners, Buyers, Assayers section. It's the only place we allow commercial advertising. I've disabled the link in your post.

Dave
 
There are too many dangerous videos out there, follow the recipes here on the forum in stead.

Edit to add:
The process is basically like this: pyrolize, incinerate, grind, magnetic separation, gravity separation, incinerate and smelt or dissolve.
You said incinerate twice. Do I burn it at two separate stages? Also, pyrolysis and incineration produce the same result re remaining metals, right? The burning will oxidize material either way?
While I'm asking, will I have a readily marketable product if I separate the char (gravity separation) and dry the product?
Thank you for all you do.
 
You said incinerate twice. Do I burn it at two separate stages? Also, pyrolysis and incineration produce the same result re remaining metals, right? The burning will oxidize material either way?
While I'm asking, will I have a readily marketable product if I separate the char (gravity separation) and dry the product?
Thank you for all you do.
Pyrolysis is to remove and safely burn the VOCs not to ash the chips.
When pyrolysisis is done there should be no smoke when ashing/incinerating the chips after.
Due to the compactness if the chips they need to be ground up and incinerated again.
Usually after gravity separating them.
When all that is done there should not be any black specks left.
If you decide to smelt them, pyrolysis is enough.
As the Carbon will combust during the smelting and will not be around during any chemical processing.
 