Hey everyone
First off California :no buchner or flasks allowed
I have what appears to be the same shape as a flask
I have tried repeatedly to build a funnel that would
allow for vacuum, but keep getting stuck on the same
spot
The air seems to suck from around my coffee filters
Instead of from the bottom, it would appear the weight
Of the liquid is not heavy enough to push the filter
against the funnel, which makes no sense since it is
a vacuum? ??
Anyways here are some. Pics
Remember this is out in the field not at home
And I do plan on getting a vacuum pump.
Thanxs Steyr223 rob
First off California :no buchner or flasks allowed
I have what appears to be the same shape as a flask
I have tried repeatedly to build a funnel that would
allow for vacuum, but keep getting stuck on the same
spot
The air seems to suck from around my coffee filters
Instead of from the bottom, it would appear the weight
Of the liquid is not heavy enough to push the filter
against the funnel, which makes no sense since it is
a vacuum? ??
Anyways here are some. Pics
Remember this is out in the field not at home
And I do plan on getting a vacuum pump.
Thanxs Steyr223 rob