Anytime you mix electricity and saturated salt water you can expect chlorine gas.

For this reason you need a well ventilated area.

Steve
 
Steve,

Thanks so much for sending the parts so quickly. Its greatly appreciated. If its okay, I have one (at least for now--LOL) silly question. When making the copper mesh basket, am I correct in believing that it is in place of the SS anode and hung on the Pyrex itself as opposed to wrapped around the SS bar?

Cheers,
John
 
John,

The bar used when you are stripping medium sized items with the clip. The copper mesh is used without the bar.

Sorry I had to change dishes on you my supplier of the others discontinued the deep dish. You should mount the bar outside the shallow dish so you don't get it in the acid.

I'm working on locating another source for the deep dishes and will send you one if i can find them.

Steve
 
Thanks Steve, I was wondering just that very thing. If one pops up, cool, but don't lose any sleep over it either way.

Cheers,
John
 
All of you are incredible smart with all of this lingo. I hope to learn all I can!!!
lazersteve you have helped alot in just one day of research. Thanks!!
 
Hello i wonder can i use a anode and catode from a automobile battery
for the cell??? :?:
 
I found a source again for the deep dishes like the one in my videos, if anyone is interested.

Steve
 
What size cups? I sell a variety of sizes of fused silica dishes on my website, the smallest of which is around 2.5" in diameter.

Steve
 

Latest posts

Back
Top