Newbie here,
Just a curious question. When reducing the solution down by heating it for a while, whats the result for acid and water quantity proportions. For example: 400ml HCL + 100ml HNO3 (AR) + 3ml H2SO4 + 200ml H2O (ice cubes) will reduce to what if I boil down the solution to 200ml? I understand the nitric will disappear making this process advantageous preventing having to use urea.
Just a curious question. When reducing the solution down by heating it for a while, whats the result for acid and water quantity proportions. For example: 400ml HCL + 100ml HNO3 (AR) + 3ml H2SO4 + 200ml H2O (ice cubes) will reduce to what if I boil down the solution to 200ml? I understand the nitric will disappear making this process advantageous preventing having to use urea.