Ahk
Well-known member
I have salt dropping with my aqua regia how do I just dissolve that so I can seperate it from the gold
Salt is a rather vague term chemically, so a description of what you did or a photo of the salt will get you back on the road to recovery.I have salt dropping with my aqua regia how do I just dissolve that so I can seperate it from the gold
I’ll post another picture after it’s all filtered off so you can seeI picked this off of the cotton filter. This is my first time trying to refine gold. It’s such an interesting process learningView attachment 66369
Thank you so much, man I really appreciate the help. Is it possible to dissolve the silver into some nitricMt first guess would be you didn't filter the solution effectively and what settled out after you dropped the gold was a mixture of Silver Chloride and Gold powder. If this is true, a soak in an ammonia solution will dissolve the Silver Chloride leaving clean gold.
The photo came in after I started typing and the chunks look like undissolved metabisulfite. If that is the case, hot water should dissolve it away.
Actually it may be a little bit of both.
silver metal dissolves in nitric, Silver Chloride does not, that requires ammonia or sodium thiosulfate.Is it possible to dissolve the silver into some nitric
Perfect thank you for helping a rookie outsilver metal dissolves in nitric, Silver Chloride does not, that requires ammonia or sodium thiosulfate.
Is there a certain concentration or will regular store brand work just finesilver metal dissolves in nitric, Silver Chloride does not, that requires ammonia or sodium thiosulfate.
This looks like ordinary coarse sand.ok so quick update tried to dissolve the salt by heating water still wouldn’t dissolve. This is what is left View attachment 66375I’m now about to heat ammonia to try and put the silver into solution
It really does it freaked me out I’ll go grab a pic of it, just a bunch of connectors and low grade pinsThis looks like ordinary coarse sand.
What is your start product?
Roger that. I followed a trinity gold video I went directly to aqua regia as per instructions, let all metals dissolve I did that step 3x, until the reactions stoppedI think you have arrived at the point where a description of what you started with and what you did next as well as when you tested and how will get you to the bottom of this quickly. If you did the ammonia, did acidifying it with Hydrochloric Acid give you indication of Silver Chloride? Having us fill in the gaps about what you did by assumption is not as definitive as you telling us the story. Sorry, we tried the quick way, now let’s do it the proper way.
Roger that. I followed a trinity gold video I went directly to aqua regia as per instructions, let all metals dissolve I did that step 3x, until the reactions stoppedView attachment 66378
Then I strained it all out rinsed it all into my bucket, resulting in thisView attachment 66379
I tested for gold and stannous came back positive for gold, I then proceeded to denox with urea. I know for a fact I used wayyy to much SMB to drop, that my good sir is how I ended up in this pickle
Enter your email address to join: