S SRM Well-known member Supporting Member Joined Aug 14, 2022 Messages 90 Location PNW US Today at 7:24 AM #21 Have you considered flotation to remove the base metals? While this would involve chemicals, they are usually small amounts of soaps and oils and designed to be removed from water systems.
Have you considered flotation to remove the base metals? While this would involve chemicals, they are usually small amounts of soaps and oils and designed to be removed from water systems.