Interesting idea, I like it. Is it designed for a continuous run?
Yes, I can feed the furnace continuously, after its full I can either slag off slags by tilting it abit or by pouring it into pyramid mold then feed again, took about only 1 hour to smelt first batch , use natural gas for first heat then use waste motor oilInteresting idea, I like it. Is it designed for a continuous run?