I had a thought... did you test the leech after the nitric only step? You mentioned that you "dipped the boards in NaOH"... im wondering if maybe some HCl was trapped in the board fibers/through holes and may have made it past the "neutralization" step. It wouldn't take much at all to dissolve 0.3g.

Just a thought.
 
mls26cwru said:
I had a thought... did you test the leech after the nitric only step? You mentioned that you "dipped the boards in NaOH"... im wondering if maybe some HCl was trapped in the board fibers/through holes and may have made it past the "neutralization" step. It wouldn't take much at all to dissolve 0.3g.

Just a thought.

Yes nitric solution was checked few times with stannous and turned out negative for gold.
 
Martijn said:
You replied to a post from 2014, in which is described a process of leaching RAM fingers in HNO3 and H2O2? Which process is that?
AP misunderstood perhaps? Try not to copy questionable and old info.

Without reading the other thread, adding H2O2 to nitric acid oxidizes the nitric oxide gases and turns it back into nitric acid. It decreases the red NOx cloud and makes your nitric acid last longer.

Göran
 