How to extract the precious metals from these relays? I thought that I would take it apart and put it in dilute nitric acid to dissolve the silver and palladium and the rest in AR. I can't wait for the iron to dissolve.
The best is to open them and separate all that is valuable from the junk. Dispose of the junkHow to extract the precious metals from these relays? I thought that I would take it apart and put it in dilute nitric acid to dissolve the silver and palladium and the rest in AR. I can't wait for the iron to dissolve.
I understand and thank you for your answer! I don't know where the palladium and silver are in it, I recognize the gold.The best is to open them and separate all that is valuable from the junk. Dispose of the junk
Then you can strip the remaining base metals from the valuables.
Why do you think there are Pd and Ag?I understand and thank you for your answer! I don't know where the palladium and silver are in it, I recognize the gold.
I understand! Thank you!Why do you think there are Pd and Ag?
All PMs will be in the contact points inside and potential the leads.
So if you strip off the leads and the contact points additionally to the pins.
You should be left with just a small amount of base metal and even less PM.
All right! It will be!Next time you take pictures, don't take them on a flowed background. I it makes it hard to see what you have. Use a plain background.
Dave
I know that gold and silver are used because they conduct electricity better than copper, I don't know why other precious metals are added.Why do you think there are Pd and Ag?
All PMs will be in the contact points inside and potential the leads.
So if you strip off the leads and the contact points additionally to the pins.
You should be left with just a small amount of base metal and even less PM.
Next time you take pictures, don't take them on a flowed background. I it makes it hard to see what you have. Use a plain background.
Dave
Welcome to us.I wanted to neutralize the nitric acid with sodium carbonate, but it didn't work out, so I cemented it with copper, and I think that's why there was iron hydroxide on top. What do you think? Why does silver not dissolve in AR?
Ammonium Chloride, Copper cementing or Zinc cementing depending completely on how it was dissolved.How can palladium be precipitated from nitric acid? 500 grams of dmg costs $320 here in our country. Do I need to detoxify the nitric acid before I precipitate it?
I haven't unlocked it yet! I want to dissolve it with 35% nitric acid.I wanted to write Denox.Ammonium Chloride, Copper cementing or Zinc cementing depending completely on how it was dissolved.
You don’t detox Nitric, it is always as toxic as it is.
But I guess you mean deNOx.
If you have dissolved it with excess Nitric I assume it is necessary.
Give us a bit more background and your questions should be easier to answer.
Ok.I haven't unlocked it yet! I want to dissolve it with 35% nitric acid.I wanted to write Denox.
I processed relays.Ok.
What material is it?
It might be done with HCl and Peroxide in stead, depending on the material.
So your plan is to dissolve Silver and Pd first and then Gold?I did not want to write this. The translator is wrong. So there are silver-plated gold-plated and palladium relays.