I'm a bit confused.
Are you trying to cupel these?
I'm using then like a melting dish it's all I had on hand to test small samples I use the crucible as a safety to catch boil over. It all failed Now I'm grinding all the failed cupels and a crucible to see if there's any gold. I'm not using any collector metal just powdered concentrate and flux. I've made a lot of gold buttons this same way there only good for one heat cycle.
 
Last edited:
I'm using then like a melting dish it's all I had on hand to test small samples I use the crucible as a safety to catch boil over. It all failed Now I'm grinding all the failed cupels and a crucible to see if there's any gold. I'm not using any collector metal just powdered concentrate and flux. I've made a lot of gold buttons this same way there only good for one heat cycle.
Ok. The use of Borax puzzled me.
 
I reground my failed attempt at smelting - jaw crusher - chain mill - Blue Bowl - panned with mercury. I may have gained a little gold and have a little dirty gold in Phosphoric Acid soaking. I need to combine and retort the amalgam and see what I have for a total weight.
 

Attachments

  • 20241215_093857.jpg
    20241215_093857.jpg
    911.5 KB
  • 20241215_101644.jpg
    20241215_101644.jpg
    1.8 MB
  • 20241215_123924.jpg
    20241215_123924.jpg
    390 KB
  • 20241215_122843.jpg
    20241215_122843.jpg
    1.8 MB
  • 20241215_123238.jpg
    20241215_123238.jpg
    1.4 MB
I reground my failed attempt at smelting - jaw crusher - chain mill - Blue Bowl - panned with mercury. I may have gained a little gold and have a little dirty gold in Phosphoric Acid soaking. I need to combine and retort the amalgam and see what I have for a total weight.
Did you roast the sulfides prior to smelting? Are you going after the Silver in the Galena?
 
Did you roast the sulfides prior to smelting? Are you going after the Silver in the Galena?
This is cleanup from our place in northern California not the Nevada ore. I still need to crush the rest of the Nevada samples before I decide. I'm roasting our ore samples as part of my sampling routine.
 
Last edited:
Nice day for a little cleanup of micro gold you never know what's hiding in a piece of quartz. 5 pounds of quartz roasted-jaw crusher-chain mill- through a stack of screens ribbed micro sluiced then panned. It takes a bunch of this to make a payday, but this rock was right next to the barn by my work area
 