Dont follow my advice, as it's only theorically, never tryed, but
If it was me...i will add NaOH and good amount of water:
Most of metal hydroxyde have very very low solubility in water. So then i will have ONLY metal hydroxyde, like Copper hydroxyde, gold hydroxyde, etc...
At least at that point no more other salt than metal. Then i will dry it to have the salt in form of powder.
Then maybe dissolve it in dilute sulfuric acid hoping that i will dissolve Copper and that gold sulfate have maybe low solubility.
If both dissolve in dilute sulfuric, then i will add SMB, hoping that SMB will precipitate the gold from the gold sulfate.
If it was me...i will add NaOH and good amount of water:
Most of metal hydroxyde have very very low solubility in water. So then i will have ONLY metal hydroxyde, like Copper hydroxyde, gold hydroxyde, etc...
At least at that point no more other salt than metal. Then i will dry it to have the salt in form of powder.
Then maybe dissolve it in dilute sulfuric acid hoping that i will dissolve Copper and that gold sulfate have maybe low solubility.
If both dissolve in dilute sulfuric, then i will add SMB, hoping that SMB will precipitate the gold from the gold sulfate.