So it took a while but I am getting there. The solution was too saturated so I refreshed it with 500ml HCl and turned on the bubbling again.
There was still about 5% gold pins on the fingers.

I rinsed it for the first time and this is the result. What a great sight to see for the first time.

IMG_6581.jpg

I collected the HCl with Copper to get the clean in a later stage.

Then I rinsed the filter with plenty of water and collected that in a separate flask.
It is light blue. Can I neutralize it and drain in through the sink or is there too much metal in there?
IMG_6584.jpg
 
So it took a while but I am getting there. The solution was too saturated so I refreshed it with 500ml HCl and turned on the bubbling again.
There was still about 5% gold pins on the fingers.

I rinsed it for the first time and this is the result. What a great sight to see for the first time.

View attachment 64968

I collected the HCl with Copper to get the clean in a later stage.

Then I rinsed the filter with plenty of water and collected that in a separate flask.
It is light blue. Can I neutralize it and drain in through the sink or is there too much metal in there?
View attachment 64969
Nice.
Just set the AP solution aside and use next time.
It lives practically for ever.
 
Nice.
Just set the AP solution aside and use next time.
It lives practically for ever.
What about the light blue solution which contains mainly of water with a little bit of left over copper solution?
Can I dispose of that through the drain after it is neutralized or is there too much metal still in it?
 
The light blue could be nickel. Do not pour it out. A large number of people are highly allergic to nickel. Treat it with your other waste solutions.
 
What about the light blue solution which contains mainly of water with a little bit of left over copper solution?
Can I dispose of that through the drain after it is neutralized or is there too much metal still in it?
Put it with the rest of your liquid waste and run it through a proper waste treatment.
The AP is not waste. ;)
 