If I have different types of silver, (i.e; oxide, chloride, sulfide, etc.) all mixed together, how can I separate them? I know what you're asking... Why would they be mixed together.? Let's just say I gotta get it all gathered up quickly, I'm limited on storage containers and time. I'd like to finish what I started at a later date. I have some silver precipitates that have been cleaned of all acids and some that are not, however even the acidic containers have all dried up. How can I do this?
 
If I have different types of silver, (i.e; oxide, chloride, sulfide, etc.) all mixed together, how can I separate them? I know what you're asking... Why would they be mixed together.? Let's just say I gotta get it all gathered up quickly, I'm limited on storage containers and time. I'd like to finish what I started at a later date. I have some silver precipitates that have been cleaned of all acids and some that are not, however even the acidic containers have all dried up. How can I do this?
Welcome to us.
You have a veritable mess on your hands that is correct.
But in order to sort it out we need to get some more info.
You said you have Silver Chloride, Silver Oxide and Silver Sulfate in a mix.
So we need to know how this came to be.
The silver Chloride, how was it created?
Silver Oxide how did that come into action?
And the Silver sulfate.

The good thing is that Silver Oxide will dissolve in Nitric.
So that may be fixed.
Dried Silver Chloride more or less have only one route and that is smelting.

So please indulge us with a more detailed description.

And we also want you to study these links:

We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/forums/safety.47/
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/dealing-with-waste.10539/

Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.33333/


Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
 