kadriver, i used Na2S2O5 as standard precipitant.the gold was double refined, source was ceramic CPUs, so main contaminant after first drop was AgCl. another contaminants were from coreduction with SMB. gold was dropped in one take from 1 liter of HAuCl4 in second refinement