Hello,
I melt my gold in house. When I make a bar, why does one side of the gold comes out smooth and the other side looks very crusty. Please take a look at the pictures. When I give this to the refinery, they drill both sides. The one with the crusty side shows a lower karat reading. I have a Thermofisher gun as well. Looking forward to the responses.
Thank you
I melt my gold in house. When I make a bar, why does one side of the gold comes out smooth and the other side looks very crusty. Please take a look at the pictures. When I give this to the refinery, they drill both sides. The one with the crusty side shows a lower karat reading. I have a Thermofisher gun as well. Looking forward to the responses.